Our TiSe2 crystals are stabilized in 2H-phase (CDW metallic phase). They are grown using two different techniques through chemical vapor transport (CVT) or flux zone growth (see description of these two methods below). These crystals are treated as gold standards in 2D materials field owing to perfected electronic behavior with guaranteed CDW response. Our TiSe2 crystals are notoriously known low impurity resistance (zero temperature resistance), high carrier mobility, extremely clean and sharp XRD peaks, and negligible amount of defects (see published results as well as CVT vs. Flux based methods below ). Our TiSe2 crystals are large in size and ready for exfoliation without any preparation. If you research needs STM grade surfaces or even STM samples (TiSe2 mounted on conductive STM holders) please contact us, we will be happy to arrange these samples.

Properties of vdW TiSe2 crystals

Growth method matters> Flux zone or CVT growth method? Contamination of halides and point defects in layered crystals are well known cause for their reduced electronic mobility, reduced anisotropic response, poor e-h recombination, low-PL emission, and lower optical absorption. Flux zone technique is a halide free technique used for synthesizing truly semiconductor grade vdW crystals. This method distinguishes itself from chemical vapor transport (CVT) technique in the following regard: CVT is a quick (~2 weeks) growth method but exhibits poor crystalline quality and the defect concentration reaches to 1E11 to 1E12 cm-2 range. In contrast, flux method takes long (~3 months) growth time, but ensures slow crystallization for perfect atomic structuring, and impurity free crystal growth with defect concentration as low as 1E9 - 1E10 cm-2. During check out just state which type of growth process is preferred. Unless otherwise stated, 2Dsemiconductors ships Flux zone crystals as a default choice.


产品咨询

留言框

  • 产品:

  • 您的单位:

  • 您的姓名:

  • 联系电话:

  • 常用邮箱:

  • 省份:

  • 详细地址:

  • 补充说明:

  • 验证码:

    请输入计算结果(填写阿拉伯数字),如:三加四=7
泰州巨纳新能源有限公司
  • 联系人:陈谷一
  • 地址:江苏省泰州市凤凰西路168号
  • 邮箱:taizhou@sunano.com.cn
  • 电话:021-56830191
联系我们

扫一扫以下二维码了解更多信息

销售微信咨询

网站二维码

版权所有©2024泰州巨纳新能源有限公司All Rights Reserved    备案号:苏ICP备17000059号-2    sitemap.xml    总访问量:58296
管理登陆    技术支持:化工仪器网